详细信息
文献类型:期刊文献
中文题名:低成本低毒脲醛树脂胶的制备
英文题名:Preparation of Low Formaldehyde Release UF Resin with Low Cost
第一作者:任一萍
机构:[1]中国林科院木材工业研究所
年份:2003
卷号:17
期号:4
起止页码:30-32
中文期刊名:木材工业
外文期刊名:China Wood Industry
收录:CSTPCD
语种:中文
中文关键词:低毒脲醛树脂胶;合成工艺;胶合板;甲醛释放量;胶合强度
外文关键词:Low toxicity urea-formaldehyde resin; Formaldehyde emission; Bonding strength
分类号:TQ433
摘要: 采用新的合成工艺,在不提高脲醛胶成本的情况下,制备低毒脲醛树脂胶,其性能达到GB/T14732-93要求,压制的胶合板力学性能好,板材甲醛释放量达到GB18580-2001中E2级水平。
A low toxicity ureaformaldehyde (UF) resin has been formulated by using a new technology without increasing the production cost. Test results showed not only the quality of the adhesive meets the requirements of National Standard GB/T 1473293, but also the bonding strength of plywood from Populus bolleana wood bonded with it is above 1.0 MPa. Furthermore, the board formaldehyde emission content also meets National Standard GB 185802001 E2 level.