X射线扫描法和切片法测量干燥过程中杉木含水率分布的比较研究 被引量:4
Comparison of X-ray scanning and slice methods for moisture distribution measurements when drying Cunninghamia lanceolata plantation wood
文献类型:期刊文献
中文题名:X射线扫描法和切片法测量干燥过程中杉木含水率分布的比较研究
英文题名:Comparison of X-ray scanning and slice methods for moisture distribution measurements when drying Cunninghamia lanceolata plantation wood
作者:余乐[1] 吕建雄[1,2] 李贤军[1] 徐康[1] 吴义强[1] 蒋佳荔[3]
第一作者:余乐
机构:[1]中南林业科技大学材料科学与工程学院;[2]中国林业科学研究院 木材工业研究所国家林业局木材科学与技术重点实验室;[3]中国林业科学研究院木材工业研究所 国家林业局木材科学与技术重点实验室
年份:2013
卷号:30
期号:4
起止页码:543-547
中文期刊名:浙江农林大学学报
外文期刊名:Journal of Zhejiang A & F University
收录:CSTPCD;;北大核心:【北大核心2011】;CSCD:【CSCD_E2013_2014】;
基金:国家杰出青年科学基金资助项目(30825034);中南林业科技大学木材科学与技术国家重点学科基金资助项目
语种:中文
中文关键词:林业工程;X射线扫描法;切片法;含水率分布;决定系数;木材干燥;杉木
外文关键词:forest engineering;X-ray scanning;slice method;moisture distribution;coefficient of determination(R2);wood drying;Cunninghamia lanceolata
分类号:S781.3
摘要:以杉木Cunninghamia lanceolata人工林木材为研究对象,分别采用X射线扫描法和切片法研究了常规干燥过程中木材内含水率分布规律,以期检验X射线扫描法的测量精度,探讨采用X射线法动态检测干燥过程中木材内含水率分布的可行性。结果表明:在各个干燥阶段,X射线扫描法测得的厚度方向各层含水率测量值与用切片法得到的含水率测量值之间无显著差异(P>0.05),且两者之间相关的决定系数在0.90以上;在整个干燥阶段,切片法测量的每层含水率值大多低于利用X射线扫描法的测量值,在含水率较高阶段(55%,46%,34%),两者之间的差值大于含水率较低阶段(26%,20%,12%,8%)。由此可见,采用X射线扫描法测量干燥过程中木材内含水率分布是切实可行的。
To test measurement accuracy of the X-ray scanning method and to explore its feasibility for determining moisture content distribution with Chinese fir plantation wood(Cunninghamia lanceolata),the X-ray scanning and slicing methods were compared during the conventional drying process.Results with the two methods for each drying stage showed no significant differences(P >0.05).In addition,a regression analysis revealed R2 > 0.90 for the two methods.During the entire drying process,the moisture content of each layer measured with the slice method was lower than the X-ray scanning method;however,differences were greater when moisture content was high.Thus,using X-ray scanning to measure the moisture content distribution of wood during the drying process would be practical.