Mechanical strength and combustion properties of biomass pellets prepared with coal tar residue as a binder ( SCI-EXPANDED收录 EI收录) 被引量:53
文献类型:期刊文献
英文题名:Mechanical strength and combustion properties of biomass pellets prepared with coal tar residue as a binder
作者:Cheng, Jun[1] Zhou, Fan[1,2] Si, Tingting[1] Zhou, Junhu[1] Cen, Kefa[1]
第一作者:Cheng, Jun
通信作者:Cheng, J[1]
机构:[1]Zhejiang Univ, State Key Lab Clean Energy Utilizat, Hangzhou 310027, Zhejiang, Peoples R China;[2]Chinese Acad Forestry, Res Inst Wood Ind, Beijing 100091, Peoples R China
年份:2018
卷号:179
起止页码:229-237
外文期刊名:FUEL PROCESSING TECHNOLOGY
收录:;EI(收录号:20182905563301);Scopus(收录号:2-s2.0-85049886095);WOS:【SCI-EXPANDED(收录号:WOS:000445316800022)】;
基金:This work was supported by National Natural Science Foundation China (51676171), National Key Research and Development Program China (2016YFB0601003), Zhejiang Provincial Natural Science Foundation - China (LR14E060002).
语种:英文
外文关键词:Coal tar residue; Biomass pellets; Binder; Mechanical strength; Combustion properties
摘要:To reutilise the hazardous waste material coal tar residue (CTR) to bring environmental and economic benefits, CTR was first used as a binder to prepare biomass pellets with enhanced mechanical strength and heating values. CTR, which mainly contained asphaltenes (40.06%), aliphatics, aromatics and non-hydrocarbon components, had a high viscosity (72,276 mPa.s) and heating value (27.46 MJ/kg). When the CTR percentage increased from 0 to 40 wt%, the abrasive resistance of wheat straw, sawdust and moso bamboo pellets significantly increased from 10.62-69.20% to 95.66-98.24%, while their water resistance time increased from 6 s to > 30 min and their heating value increased by 20.62-25.96%. The ignition temperature of wheat straw pellets increased from 275.7 to 280.7 degrees C as the CTR content increased from 0 to 30 wt%, whereas the maximum burning rate decreased from 1.28 to 0.82 mg/min and the burnout temperature increased from 465.33 to 563.33 degrees C.